Significant comparison of stainless steel pipes before and after polishing

Problems encountered by customers

  • A Colombian industrial manufacturer pointed out that hand and mechanical polishing left uneven “orange peel” texture and micropits on large areas of stainless steel, failing to meet hygiene and corrosion resistance standards.
  • Welds and heat-affected zones require multiple grinding/polishing processes, and visible transition lines and residual abrasive pose a risk of contamination to food-grade equipment.
  • Poor batch consistency: Up to 35% of parts require rework, causing production delays of 3-4 days per order.

Weshining’s solution

  • Delivered a uniform, defect‑free ≤0.02 μm Ra finish across entire surfaces, including welded joints and complex curvature, with no orange peel or pitting.
  • Reduced polishing time from 90 min to 12 min per large component – 87% faster, eliminating multi-stage handwork.
  • Achieved 100% first‑pass quality; eliminated rework and contamination risks, increasing the manufacturer’s output by 40% without adding labor.
01 %E5%85%B6%E4%BB%96EN 01 1 Significant comparison of stainless steel pipes before and after polishing
Case Album
Related
  • Before and after polishing of stainless steel drill bits
  • Stainless steel detail before and after polishing comparison
  • Comparison of hardware workpieces before and after polishing
  • Significant comparison of stainless steel pipes before and after polishing

Contact us for:

Let Weshining supercharge your polishing process. Turn rough pieces into mirror – finish masterpieces — efficiently, affordably, and flawlessly!

Get an instant quote

Please fill out the form to send us message, we will get back to you within 2-3 hours on business hours.